Montažna proga
tip izdelka
|
Metode | Enote | Pogoji | Rezultati | Zahteve | Uspešno/neuspešno |
Natezne lastnosti
|
EN 12230
|
Mpa
|
Novo, 23 ° C | 0,54 | > 0,40
|
Pass |
Po A/W staranju (1) | 0,55 | Pass | ||||
Po Spike Resistance ⑵ | 0,50 | Pass | ||||
Po A/W staranju (1) + Odpornost na konice (2) | 0,49 | Pass | ||||
Različica (%)
|
Po Spike Resistance ⑵ | 7 | <20
|
Pass | ||
Po A/W staranju (1) +
Spike Resistance ⑵ |
11 | Pass | ||||
Raztezek pri pretrganju
|
EN 12230
|
%
|
Novo, 23 ° C | 61 | > 40
|
Pass |
Po staranju ⑴ | 52 | Pass | ||||
Po Spike Resistance ⑵ | 70 | Pass | ||||
Po A/W staranju ⑴ + odpornost na konice ⑵ | 42 | Pass | ||||
Različica (%)
|
Po Spike Resistance ⑵ | 15 | <20
|
Pass | ||
Po A/W staranju (1) + Odpornost na konice ⑵ | 19 | Pass | ||||
Odpornost proti obrabi | EN ISO 5470-1 | g | Novo, 23 ° C | 2.8 | <4,0 izgube mase med 500 in 1500 cikli | Pass |
Prepustnost vode | EN 12616 | mm/h | Novo, 23 ° C | > 2 000 | > 150 mm/h | Pass |
Absolutna debelina | EN 1969 (metoda A) | mm | Novo, 23 ° C | 13,0 | > 10 | Pass |
Skupna debelina | EN 1969 (metoda A) | mm | Novo, 23 ° C | 13.6 | - | - |
Dimenzije
(1) A/ W staranje - staranje vročega zraka + staranje tople vode
Staranje vročega zraka in vode poteka po standardu EN 13817 in takoj po njem po standardu EN 13744. Po izpostavljenosti površini se ponovno preverijo naslednje lastnosti, da se preveri morebitna sprememba:
Absorpcija udarcev
Natezne lastnosti / Raztezek pri lomu
(2) Odpornost na konice
Preskus odpornosti na konice se izvede po preskusni metodi, opisani v standardu EN 14810.